HASTELLOY C-276
Nickel-Molybdenum-Chromium Alloy. Values below are the requirements of the standard named beside them; the mill certificate governs the material delivered.
Designations
- UNS
- N10276
- EN number
- 2.4819
- EN name
- NiMo16Cr15W
Density
- Density
- 8890 kg/m³
- Per
- Special Metals / nickel alloy datasheets
- Corrosion resistance
- Excellent
- Product forms
- Sheet, plate, bar, pipe
Chemical composition
| Standard | Product form | Basis | C | Si | Mn | S | Cr | Mo | Other rules |
|---|---|---|---|---|---|---|---|---|---|
| ASTM / Haynes-type reference | Ni-Mo-Cr-W | Specification | ≤ 0.01 | ≤ 0.08 | ≤ 1 | ≤ 0.03 | 14.5–16.5 | 15–17 | W 3.0-4.5; Fe 4.0-7.0; Co max 2.5; V max 0.35; Ni balance |
mass %. A blank cell means the standard sets no requirement for that element, not zero. Single values are limits: "≤" a maximum, "≥" a minimum.
Reference values from the cited standards. They describe what the standard requires, not a specific heat of material; the mill test certificate governs what is delivered.
Mechanical properties
| Standard | Product form | Condition / temper | Test temperature | Yield | Tensile | Elongation min | Notes |
|---|---|---|---|---|---|---|---|
| ASTM B575/vendor reference | Plate/Sheet | Solution heat treated | 20 °C | 0.2% offset ≥ 283 MPa | ≥ 690 MPa | 40 % (Product/condition dependent) | Representative minimums. |
Each row is one standard, one product form and one condition — the values do not transfer across rows. A blank cell means the standard sets no requirement.
Reference values from the cited standards. They describe what the standard requires, not a specific heat of material; the mill test certificate governs what is delivered.
Physical properties
| Temperature | Density | Young’s modulus | Poisson’s ratio | Thermal expansion (20–100°C) | Thermal conductivity (20°C) | Specific heat | Electrical resistivity (20°C) | Melting range | Magnetic |
|---|---|---|---|---|---|---|---|---|---|
| 20 °C | 8890 kg/m³ | 205 GPa | 0.31 | 11.2 µm/m·°C | 10.2 W/m·K | 0.427 kJ/kg·°C | 1.3 µΩ·m | 1325–1370 °C | Non-magnetic |
Reference values from the cited standards. They describe what the standard requires, not a specific heat of material; the mill test certificate governs what is delivered.
Typical applications
Severe chemical corrosion, pollution control
Approximate equivalents
Approximate equivalents: equivalents are a technical reference, not a substitution instruction, verify against project specification.
| Grade | Systems | Relationship | Note | Key difference |
|---|---|---|---|---|
| HASTELLOY C-276 | UNS/ASTM → EN | Same grade, another designation | Commonly cross-referenced alloy family. | Confirm product specification. Compared designation: 2.4819 / NiMo16Cr15W. |
Common questions
- 01What is the density of HASTELLOY C-276?
- 8890 kg/m³ — the figure the weight calculators on this site use for HASTELLOY C-276. The value is Special Metals / nickel alloy datasheets’s.
- 02What is the chemical composition of HASTELLOY C-276?
- C ≤ 0.01, Si ≤ 0.08, Mn ≤ 1, S ≤ 0.03, Cr 14.5–16.5, Mo 15–17, in mass %, to ASTM / Haynes-type reference. An element the standard sets no requirement for is left blank here rather than written as zero.
- 03What are the mechanical properties of HASTELLOY C-276?
- Tensile ≥ 690 MPa, Yield ≥ 283 MPa, Elongation min ≥ 40 % — ASTM B575/vendor reference, Plate/Sheet, Solution heat treated. Those are the standard’s requirements; the mill test certificate governs the metal delivered.
- 04What is HASTELLOY C-276 used for?
- Severe chemical corrosion, pollution control